Normal strength: Yield stress is about 240 MPa, tensile strength about 360 MPa. •. High strength: Yield stress is about 340 MPa, tensile strength about 470 MPa.
Strenx® 1300 is an ultra-high-strength structural steel with a minimum yield strength of 1300 MPa. Typical applications include load-carrying structures
The new European unified technical design rules for steel structures in Eurocode 3 are applicable to steels S235 to S460. It is intended to extend these
There is an increasing demand for high strength steel in the construction of buildings and civil engineering structures. However, there is a significant